• After spraying, allow the paint to settle for about

10 minutes, then force dry with an infrared lamp.

NOTE: Follow the paint manufacturer's instructions.

Body parts being dried with an

industrial dryer can get hot enough to cause injury. Do

no touch parts being dried.

21. Polishing/buffing

• Let the paint dry gradually, then polish the surface

carefully using a polishing compound and sponge

buffing pad.

• To remove lint or dirt, wet sand the surface with

#2000 paper or finer first, then polish with

compound.

NOTE: Polish all roughness caused by sanding thor-

oughly. To do this, first polish with very fine com-

pound, then with ultra fine compound.

• After polishing, remove the masking paper and tape,

and wash the entire vehicle thoroughly.

Main Menu

Table of Contents

NH-585P (Cayman White
Pearl) Paint

Color Matching

Repair of NH-585P (Cayman White Pearl) paint coat requires

different procedures from that of metallic and pearl paint

coats.

Determination of color:

1. Using a #800 - #1000 sandpaper, sand the damaged paint

coat until the intermediate coat 2 appears.

2. Polish the exposed paint coat with an ultra fine com-

pound, then compare its color with the color sample

provided.

3. Prepare a paint based on the color sample selected

according to the instructions.

4. After preparing, check that the paint prepared matches

the color sample selected in step 2.

NOTE: On pearl paint, the color of the intermediate coat 2

will determine the final color of the paint repair.

Main Menu

Table of Contents

NH-585P (Cayman White Pearl) Paint

Color Matching (cont'd)

Mixing (Reference):

The paint prepared should be mixed with thinner and hard-

ner as follows.

NOTE: The following examples are based on the paints

manufactured by ISAM Paint Co., Ltd High Art #3000).

PAINT (Intermediate Coat 2: color base)

2. Pour the mixture through a filter, then spray 2-3 light

coats over the damaged surface.

NOTE: Spray the mixture until the intermediate coat 2

is thoroughly covered.

3. Prepare paint for graduation by mixing 1 part of

Paint with 19 parts of the paint (B). Stir the mixture

well.

4. Pour the mixture through a filter, then spray 2-3 light

coats of the filtered mixture over paint Start at the center,

then work toward the edge.

NOTE:

• Check that the painted coat matches the color

of the body paint while spraying.

• Application of the mixture will determine the final

color of the paint repair. Do not spray the mixture

excessively as this may alter the final color of the

repair.

5. Apply 1-2 light coats of paint over the repaired

surface.

6. For the final top coat, add 15% thinner to a 4 : 1

mixture of the clear paint and hardener.

The above paints and materials or their equivalents should

be used.

NOTE: Follow the paint manufacturer's instructions when

mixing the paint and other materials.

Refinishing Procedures:

7. Spray 2-3 light final top coats over the damaged area.

• Ventilate when spraying paint. Most paint contains

substances that are harmful if inhaled or swallowed. Read

the paint label before opening paint container.

• Avoid contact with skin. Wear an approved respirator,

gloves, eye protection and appropriate clothing when

painting.

• Paint is flammable. Store in a safe place, and keep it

away from sparks, flames or cigarettes.

1. To prepare the first coat (paint ) add a 1 part of

paint to 1 part of paint and mix well.

Main Menu

Table of Contents

Soft Chipping Guard Primer Coat

General

The removal of paint and Undercoating by stones and gravel immediately exposes metal to the atmosphere, causing it to rust. The

thickness of this rust increases if the process continues unchecked. The soft chipping guard primer protects against damage due

to the impact of flying objects. The purpose of this guide is to provide information you will find useful when repairing damage to

the protective coating. Refer to the Soft Chipping Primer Undercoating Diagram.

The soft chipping guard primer is applied over the E.D. (Electrostatically Deposited) primer. It is followed by guide coating and top

coating.

The soft chipping guard primer produces a smooth surface when dry. It should be sprayed so the thickness of the protective film

is 20 microns.