12.13.4.3 Deep Polishing Treatment Process Example 

1.  Sand the surface with a piece of 2000# sanding 

paper. Press the sanding paper very close to the 
surface and sand in circles. 

 

NL12-1003b

2.  Remove the polishing power from the surface. 

 

NL12-1000b

3.  Apply an appropriate amount of polishing wax to 

the surface and adjust the polishing machine 
speed. 

 

NL12-1005b

 

2843

 
 

 

4.  Put the wool ball onto the surface, turn on the 

machine with a speed at 2,500-3,000 r/ min. 

Notes: 

During operation, keep the machine stable and move 
gently. Do not polish too long. Keep the polishing 
time as short as possible (3-5s), and the polishing area 
as small as possible. 

 

NL12-1004b

5.  Wet sufficiently the sponge and remove 

excessive moisture by compressing it. Apply a 
small amount of polishing wax to the surface to 
be polished and start the engine to a RPM of 2, 
500-3,000r/min after pressing the    sponge to the 
surface to be polished.    Then, slightly press for 
3-5s for polishing treatment. 

Notes: 

During operation, keep the machine stable and move 
gently. Do not operate too long to avoid overheating, 
as the paint will be damaged by the heat. 

 

NL12-1002b

 

2844

 
 

12.13.4.4 Spray Paint Process of Rigid Surface 

Take the fender for example to describe the local 
spray finishing (painting make-up) process 

Notes: 

All paint repairs for rigid surface must comply with 
Geely standards.    Confirm the repair area and select 
the repair range, such as the local repair, the whole 
repair and the whole vehicle repair. 

If the damages are caused due to the collision, the 
vehicle will be repaired by metal plate process and 
then the corresponding repair will be carried out or 
painting will be performed after the replacement of 
the parts. 

1.  For serious fender scratches, use the partial paint 

spray (repair) process. 

NL12-1006b

2.  Sand the damaged surface with a piece of P500# 

wet sanding paper in circles. 

 

NL12-1007b

3 .    Clean the surface with the degreasing agents after 

polishing. 

 

NL12-1008b

 

2845

 
 

 

4.  For primer painting, control the painting area. 

Gradually paint the edges. Do not overlap the 
paint. 

 

NL12-1009b

5.  Leave the surface dry 4-5 min and then heat to 

dry 20-30 min. 

Paint room temperature 70-80℃ (158-176 ºF) 

 

NL12-1010b

6.  After drying, sand the surface with a piece of 

P800-1,000# sanding paper. 

 

NL12-1011b